名称 |
分子量 |
粘性 |
用途 |
Tg [℃] |
Tm [℃] |
末端基 |
RESOMER L 206 S
Poly(L-lactide) |
-- |
0.8 - 1.2 |
Medical Device |
60 - 65 |
180 - 185 |
alkyl ester |
RESOMER R 202 S
Poly(D,L-lactide) |
10,000 -
18,000 |
0.16 - 0.24 |
Controlled Release |
38 - 42 |
amorphous |
alkyl ester |
RESOMER R 202 H
Poly(D,L-lactide) |
10,000 -
18,000 |
0.16 - 0.24 |
Controlled Release |
44 - 48 |
amorphous |
free carboxylic acid |
RESOMER R 203 S
Poly(D,L-lactide) |
18,000 -
28,000 |
0.25 - 0.35 |
Controlled Release |
46 - 50 |
amorphous |
Alkyl ester |
RESOMER R 203 H
Poly(D,L-lactide) |
18,000 -
28,000 |
0.25 - 0.35 |
Controlled Release |
48 - 52 |
amorphous |
free carboxylic acid |
RESOMER RG 502
Poly(D,L-lactide-co-glycolide) 50:50 |
7,000 -
17,000 |
0.16 - 0.24 |
Controlled Release |
42 - 46 |
amorphous |
alkyl ester |
RESOMER RG 502 H
Poly(D,L-lactide-co-glycolide) 50:50 |
7,000 -
17,000 |
0.16 - 0.24 |
Controlled Release |
42 - 46 |
amorphous |
free carboxylic acid |
RESOMER RG503
Poly(D,L-lactide-co-glycolide) 50:50 |
24,000 -
38,000 |
0.32 - 0.44 |
Controlled Release |
- |
amorphous |
alkyl ester |
RESOMER RG 503 H
Poly(D,L-lactide-co-glycolide) 50:50 |
24,000 -
38,000 |
0.32 - 0.44 |
Controlled Release |
44 - 48 |
amorphous |
free carboxylic acid |
RESOMER RG504
Poly(D,L-lactide-co-glycolide) 50:50 |
38,000 -
54,000 |
0.45 - 0.60 |
Controlled Release |
- |
amorphous |
alkyl ester |
RESOMER RG 504 H
Poly(D,L-lactide-co-glycolide) 50:50 |
38,000 -
54,000 |
0.45 - 0.60 |
Controlled Release |
46 - 50 |
amorphous |
free carboxylic acid |
RESOMER RG505
Poly(D,L-lactide-co-glycolide) 50:50 |
54,000 -
69,000 |
0.61 - 0.74 |
Controlled Release |
- |
amorphous |
alkyl ester |
RESOMER RG 653 H
Poly(D,L-lactide-co-glycolide) 65:35 |
24,000 -
38,000 |
0.32 - 0.44 |
Controlled Release |
46 - 50 |
amorphous |
free carboxylic acid |
RESOMER RG 752 H
Poly(D,L-lactide-co-glycolide) 75:25 |
4,000 -
15,000 |
0.14 - 0.22 |
Controlled Release |
42 - 46 |
amorphous |
free carboxylic acid |
RESOMER RG 756 S
Poly(D,L-lactide-co-glycolide) 75:25 |
76,000 -
116,000 |
0.71 - 1.0 |
Controlled Release |
49 - 55 |
amorphous |
alkyl ester |
RESOMER RG858 S
Poly(D,L-lactide-co-glycolide) 85:15 |
190,000 -
240,000 |
1.3 - 1.7 |
Controlled Release |
- |
amorphous |
alkyl ester |
RESOMER X
Polydioxanone |
-- |
1.5 - 2.2
(0.1% in HFIP, 30℃) |
Medical Device |
-10 -
-5 |
110 - 115 |
-- |